Table unit for the investigation of the creep behaviour of different materials
Tensile stress range 5...25N/mm²
Position measurement gauge 0...10mm, resolution 0.01mm
Experiments above or below room temperature possible with conditioning box
Flat specimens made of lead and PE
Specimen cross-section 2x5mm, measured length 25mm.
Specimen
Material: lead, PE
Measured length: 25mm
Tensile stress range: 5...25N/mm²
Cross-section: 2x5mm
Position measurement
Resolution 0.01mm
Range: 0...10mm.
Request a custom quote, full technical datasheet, or place a bulk / tender enquiry. Our specialists will get back to you within 1 business day with pricing, lead time, and export documentation.
As one of India's leading Creep Testing Unit manufacturers, suppliers & exporters, we deliver tender-grade quality with documented compliance to institutions, laboratories & training facilities across 65+ countries.
Every Creep Testing Unit unit is manufactured to international quality standards and tested before dispatch. Full QC documentation & calibration certificates included.
Established export channels across Africa, Asia, the Middle East & beyond. Complete shipping documentation — certificates of origin, packing lists, test certificates, customs paperwork.
Need a specific configuration of Creep Testing Unit? We offer customisation for tender specifications, OEM branding, voltage variants & bulk institutional orders.
Technical consultation before purchase, installation guidance, operator training documentation, and responsive after-sales support — backed by our specialist engineering team.
Trusted by institutions, governments & industries worldwide for reliable, tender-documentation-ready supply.
We supply Creep Testing Unit across seven major buyer segments worldwide:
Practical laboratory training & coursework experiments
STEM education & physics / chemistry / biology demos
Process quality, testing & calibration requirements
Clinical lab, diagnostics & pathology applications
Ministry, defence research & PSU lab infrastructure
UNICEF, WHO, UNDP & bilateral aid procurement
Skill development & technical training labs
Direct & sub-contractor tender fulfilment
Manufacturing scale & global reach
Documentation-ready supply for tender-grade procurement — certificates of origin, test certificates, calibration data & compliance matrices.
Laboratory Instrument India is a recognised manufacturer, supplier and exporter of Creep Testing Unit from India. We supply this product across our complete export network — from individual institutional purchases to large-scale tender supply contracts.
Nigeria, Kenya, Ghana, Ethiopia, Tanzania, Uganda, South Africa, Egypt, Morocco, Algeria, Senegal, Cameroon
Bangladesh, Sri Lanka, Nepal, Myanmar, Vietnam, Indonesia, Philippines, Malaysia
UAE, Saudi Arabia, Oman, Qatar, Kuwait, Iraq, Jordan
All shipments include complete export documentation, customs paperwork & freight handling.
Common questions from buyers, procurement officers & technical evaluators about ordering, customisation, lead time & documentation.
Speak directly with a product specialist for technical clarifications, custom configurations & bulk tender pricing.